MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
3D Systems Accura® SL 5530 High temperature resistant Stereolithography material
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Features:
  • High temperature resistance
  • Very high throughput material
  • Good water resistance
  • Suitable for under-the-hood applications
  • Suitable for electrical applications
  • Resistant to automotive fluids

Information provided by 3D Systems

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.19 g/ccLiquid
 1.25 g/ccSolid
Viscosity 210 cP
@Temperature 30.0 °C
 270 cP
@Temperature 28.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 88ASTM D 2240
Tensile Strength 57.0 - 63.0 MPaASTM D638
Elongation at Break 2.7 - 4.4 %ASTM D638
Tensile Modulus 2854 - 3130 MPaASTM D638
Flexural Strength 109 - 120 MPaASTM D 790
Flexural Modulus 2972 - 3392 MPaASTM D 790
Impact 21[J/m]; ASTM D 256
Penetration 5.5[mils]
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 68.0 °CASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 56.0 °CASTM D 648
Glass Transition Temp, Tg 82.0 °C
 
Descriptive Properties
ColorClear Amber
Critical Exposure (Ec)7.5 mJ/cm3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAPPR3148 / 239116

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.