Pyrotek offers a variety of vacuum formed products composed from Al-Therm 2100H. These alumina-silicate fibers feature a unique inorganic binder system and are custom designed to shapes which are formed to near net size. Applications - Trough liners and launders
- Distribution pan linings
- Tundishes and pouring basins
- Hot top casting components
Advantages - Excellent insulating properties
- Light-weight and low density
- Excellent resistance to molten aluminum
- Good erosion resistance
- Highly resistant to thermal shock
- No preheating required
- Easy to install and maintain
Information provided by Pyrotek. |