This material has been rebranded as a part of the NAECO® ELKON® product line. ELKONITE® 2088 has a very high refractory content and is not considered in the normal family of make and break contacts. It is used in special applications where weight or hardness together with corrosion resistance may be of primary importance. It has also found use as a rocket nozzle material. Information provided by CMW Inc. |