HumiSeal® UV40 Gel is a single component, high solids, UV curable gel. A secondary moisture cure mechanism will cure unexposed areas within 7 days at ambient conditions. The gel fluoresces under UV light to allow inspection. HumiSeal® UV40 Gel is in full compliance with the RoHS Directive 2011/65/EU.Information provided by Chase Electronic Coatings. |