MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
INEOS Styrolution K-Resin® DK11 Styrene Butadiene Copolymer (SBC)
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene-Butadiene Copolymer, SBC

Material Notes: K-Resin® DK11 makes a clear, stiff, very tough, high gloss film suitable for applications such as candy twist wrap, shrink sleeves and overwrap. K-Resin® SBC grades designed for blown film extrusion is DK11. Excellent Clarity, High Surface Gloss, Good Heat Sealability. Applications: Medical Packaging, Produce Packaging, Twist Wrap, Lidstock and Labeling Film

Information provided by Styrolution.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.02 g/ccISO 1183
Water Absorption at Saturation 0.070 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0030 - 0.010 cm/cmISO 294-4
Melt Flow 7.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ISO 868
Tensile Strength, Yield 25.0 MPaISO 527
Elongation at Break 170 %ISO 527
Elongation at Yield 2.0 %ISO 527
Tensile Modulus 1500 MPaISO 527
Flexural Strength 30.0 MPaISO 178
Flexural Modulus 1500 MPaISO 178
Charpy Impact Unnotched NB
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 1.00 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear 60.0 - 90.0 µm/m-°CISO 11359
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 62.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 52.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 84.0 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.57Sodium D Line; ISO 489
Haze 1.0 %ASTM D 1003
Transmission, Visible 92 %
@Wavelength 550 nm
ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
A. Schulman Diamond SBS 1031 Clear Styrene Butadiene Copolymer
INEOS Styrolution K-Resin® KR03 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR01 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR38 Styrene Butadiene Copolymer (SBC)
INEOS Styrolution K-Resin® KR05 Styrene Butadiene Copolymer (SBC)

PSTYR9873 / 216100

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.