MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Estane® 2103-85AE Thermoplastic Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Formerly Pellethane

Feature: Film and profile resin

Available in Americas, Europe, Middle East, Africa, India and Asia

Data provided by Lubrizol

Lubrizol acquired the Pellethane product line from Dow in 2009.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.14 g/ccASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.00 - 0.0060 cm/cmASTM D955
Melt Flow 24 g/10 min
@Load 8.70 kg,
Temperature 224 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 88ASTM D2240
Hardness, Shore D 48ASTM D2240
Tensile Strength, Ultimate 32.0 MPaASTM D412
Elongation at Break 560 %ASTM D412
50% Modulus 0.00550 GPa
@Strain 50 %
ASTM D412
100% Modulus 0.00690 GPa
@Strain 100 %
ASTM D412
300% Modulus 0.0121 GPa
@Strain 300 %
ASTM D412
Tear Strength 82.3 kN/mDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 5.0H22 Wheel, 1000g; ASTM D1044
Compression Set 25 %
@Temperature 25.0 °C,
Time 79200 sec
ASTM D395, Method B
 80 %
@Temperature 70.0 °C,
Time 79200 sec
ASTM D395, Method B
Tensile Set 80 %Elongation set after break; ASTM D412
 
Thermal PropertiesOriginal ValueComments
CTE, linear 169 µm/m-°C
@Temperature 20.0 °C
ASTM D696
Vicat Softening Point 67.2 °C120°C/hr, 9.8N; ASTM D1525
Glass Transition Temp, Tg -38.0 °C
 
Processing PropertiesOriginal ValueComments
Melt Temperature 182 - 199 °CExtrusion
 188 - 204 °CMolding
Mold Temperature 16.0 - 60.0 °C
Drying Temperature 82.0 - 93.0 °Cair dew point <-40°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer
Lubrizol Estane® 2102-55D Thermoplastic Polyurethane Elastomer
Lubrizol Advanced Materials Pearlcoat® Activa D198K Thermoplastic Polyurethane Elastomer
Huntsman IROGRAN® A 85 D 5001 Polyester-Based TPU-Injection Extrusion Grade

PDW271a / 138265

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.