MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
AISI Type A4 Tool Steel
Categories: Metal; Ferrous Metal; Tool Steel; Air-Hardening Steel; Cold Work Steel

Material Notes: High hardenability, high degree of dimensional stability in heat treatment, good wear resistance, fatigue life, toughness, and deep hardening qualities. Applications include cold forming, blanking and bending dies, forming rolls, drill bushings, knurling tools, master dies and gages.

Key Words: AISI Medium-Alloy, Air-Hardening Tool Steels A4, UNS T30104, ASTM A681, FED QQ-T-570
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.03 g/cc(A6)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 63as air quenched from 845°C, 61 HRC at 150°C temper, 60 HRC at 205°C temper, 59 HRC at 260°C temper, 58 HRC at 315°C temper, 57 HRC at 370°C temper, 56 HRC at 425°C temper, 54 HRC at 480°C temper, 53 HRC at 540°C temper, 50 HRC at 595°C temper, 40 HRC at 650°C temper.
Bulk Modulus 160 GPaTypical for steels.
Machinability 65 %Based on Carbon tool steel.
Shear Modulus 80.0 GPaTypical for steels.
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.95 - 1.05 %
Chromium, Cr 0.90 - 2.2 %
Iron, Fe 92.6 - 95.4 %as remainder
Manganese, Mn 1.8 - 2.2 %
Molybdenum, Mo 0.90 - 1.4 %
Phosphorus, P <= 0.030 %
Silicon, Si <= 0.50 %
Sulfur, S <= 0.030 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type A2 Tool Steel
AISI Type A3 Tool Steel
AISI Type A5 Tool Steel
AISI Type A7 Tool Steel
AISI Type A6 Tool Steel

MSTA4A / 14097

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.