3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy Adhesive
Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
8000
-
14000
cP
8000
-
14000
cP
Accelerator
20000
-
50000
cP
20000
-
50000
cP
Base
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
75 - 80
75 - 80
Shear Strength
0.689
MPa
100
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Neoprene/Steel
0.827
MPa
120
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Neoprene/Steel
0.965
MPa
140
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, SBR/Steel
1.03
MPa
150
psi
Overlap, Isopropyl Alcohol Wipe surface prep, SBR/Steel
1.52
MPa
220
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
2.07
MPa
300
psi
Overlap, Isopropyl Alcohol Wipe surface prep, ABS
2.28
MPa
330
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic
2.41
MPa
350
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, PVC
2.76
MPa
400
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polycarbonate
3.10
MPa
450
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene
3.28
MPa
475
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene
3.45
MPa
500
psi
Overlap, Isopropyl Alcohol Wipe surface prep, PVC
3.45
MPa
500
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polycarbonate
3.96
MPa
575
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, ABS
5.52
MPa
800
psi
Overlap, Isopropyl Alcohol Wipe surface prep, FRP
6.89
MPa
1000
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol Wipe surface prep, FRP
9.65
MPa
1400
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Phenolic
9.65
MPa
1400
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Phenolic
13.8
MPa
2000
psi
Overlap, Galvanized Steel Okite degrease Hot dip
14.5
MPa
2100
psi
Overlap, Galvanized Steel Okite degrease Electrodeposited
19.3
MPa
2800
psi
Overlap, CRS MEK/abrade/MEK
22.1
MPa
3200
psi
Overlap, Aluminum Oakite degrease
24.1
MPa
3500
psi
Overlap, Aluminum MEK/abrade/MEK
24.1
MPa
3500
psi
Overlap, CRS Oakite degrease
27.6
MPa
4000
psi
Overlap, Copper MEK/abrade/MEK
27.6
MPa
4000
psi
Overlap, Brass CDA 260
27.6
MPa
4000
psi
Overlap, Stainless Steel MEK/abrade/MEK
29.0
MPa
4200
psi
Overlap, Brass Cartridge
31.0
MPa
4500
psi
Overlap, Aluminum Etched
31.0
MPa
@Temperature 23.0 °C
4500
psi
@Temperature 73.4 °F
Aluminum, Overlap
31.0
MPa
@Temperature -55.0 °C
4500
psi
@Temperature -67.0 °F
Aluminum, Overlap
1.52
MPa
@Temperature 121 °C,
Time 900 sec
220
psi
@Temperature 250 °F,
Time 0.250 hour
Aluminum, Overlap
4.83
MPa
@Temperature 82.0 °C,
Time 900 sec
700
psi
@Temperature 180 °F,
Time 0.250 hour
Aluminum, Overlap
6.89
MPa
@Time 1800 sec
1000
psi
@Time 0.500 hour
Aluminum, Overlap
9.65
MPa
@Time 3600 sec
1400
psi
@Time 1.00 hour
Aluminum, Overlap
17.2
MPa
@Time 14400 sec
2500
psi
@Time 4.00 hour
Aluminum, Overlap
Peel Strength
4.38
kN/m
25.0
pli
7.01
kN/m
40.0
pli
T-Peel, CRS MEK/abrade/MEK, 5-8 mil bondline
8.77
kN/m
50.0
pli
T-Peel, CRS Oakite degreased, 5-8 mil bondline
10.5
kN/m
60.0
pli
T-Peel, Etched Aluminum, 17-20 mil bondline
0.526
-
0.877
kN/m
@Temperature 82.0 °C
3.00
-
5.00
pli
@Temperature 180 °F
Aluminum, T-Peel
0.877
-
1.75
kN/m
@Temperature -55.0 °C
5.00
-
10.0
pli
@Temperature -67.0 °F
Aluminum, T-Peel
10.5
kN/m
@Temperature 23.0 °C
60.0
pli
@Temperature 73.4 °F
Aluminum, T-Peel
Electrical Properties
Metric
English
Comments
Volume Resistivity
2.40e+14
ohm-cm
2.40e+14
ohm-cm
ASTM D257
Dielectric Strength
43.3
kV/mm
1100
kV/in
ASTM D149
Thermal Properties
Metric
English
Comments
CTE, linear
59.0
µm/m-°C
32.8
µin/in-°F
Below Tg
159
µm/m-°C
88.3
µin/in-°F
Above Tg
Thermal Conductivity
0.180
W/m-K
@Temperature 45.0 °C
1.25
BTU-in/hr-ft²-°F
@Temperature 113 °F
Descriptive Properties
Appearance
Amber
Accelerator
Opaque, off-white
White
Base
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
PMM34647 / 169394
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.