System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
INEOS Styrolution Lustran® SMA 244 Styrene Maleic Anhydride (SMA)
Categories:
Polymer
;
Thermoplastic
;
SMA Polymer
Material Notes:
Features: High heat resistance, Applications: Paper sizing, Pigment binder/ dispersant aid, Adhesion promoter, Compatibilizer, Ink additive
Information provided by Styrolution.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Melt Flow
10
g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D 1238
Optical Properties
Original Value
Comments
Haze
2.5 %
ASTM D 1003
Processing Properties
Original Value
Comments
Melt Temperature
250
-
270
°C
Mold Temperature
60.0
-
82.0
°C
Drying Temperature
82.0
-
93.0
°C
@Time 7200 - 10800 sec
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
NOVA Chemicals Dylark® 378P12 Glass Reinforced Engineering Resin
Lubrizol Pellethane® 2363-80A Thermoplastic Polyurethane Elastomer
Lubrizol LifeSciences Tecoflex® EG-93A TPU - Clear
BYK PRIEX® 15005 Maleic Anhydride modified LDPE
A. Schulman ComAlloy Hiloy® 261 Glass Reinforced, Modified SMA
PSTYR9910 / 216134
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.