MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Trinseo Modifier A SB Latex
Categories: Polymer; Thermoplastic; Styrene-Butadiene

Material Notes: The use of latex as a performance-enhancing additive in modified concrete systems is a proven technology. Bridge decks, highway overlays, parking decks and other structures benefit not only from the increased durability and resistance to permeation offered by latex, but also lower maintenance and total costs compared to repair alternatives. Trinseo Modifier A™/NA Latex – formerly offered by The Dow Chemical Company and Dow Reichhold Specialty Latex – has long been the performance and value leader for modified concrete. B

Product Information: Trinseo Modifier A™/NA Latex is a concrete modifier manufactured to meet latex specifications and concrete performance requirements of the Federal Highway Administration (FHWA). Conforms to Report No. FHWA-RD-78-35 “Styrene-Butadiene Latex Modifiers for Bridge Deck Overlay Concrete.”

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 47.9 %47.9 %
Particle Size 1890 µm1890 µm
Particle Mesh Size 100 Mesh100 Meshper 900 gm, <0.02%
pH 10.310.3
Surface Tension 27 dynes/cm27 dynes/cm
 
Chemical PropertiesMetricEnglishComments
Butadiene Content 36 %36 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDWST202 / 142411

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.