MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RAMPF RAKU-TOOL® RS-9225 Tin Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: 215A Tin Silicone

Key Properties:

  • High Strength
  • Low Durometer
  • Minimal Shrinkage
  • Easy 10:1 Mix
Applications:
  • Room temperature hand batch processing
  • Hobby and arts projects
  • Rapid prototyping rollers
  • Mold making
Cure: 7 days @ 77°F (25°C)

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.990 g/cc0.0358 lb/in³Activator; ASTM D-792
 1.10 g/cc0.0397 lb/in³ASTM D-792
 1.15 g/cc0.0415 lb/in³Silicone; ASTM D-792
Viscosity 125 cP125 cPActivator; ASTM D-2393
 24500 cP24500 cPMixture; ASTM D-2393
 33000 cP33000 cPSilicone; ASTM D-2393
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 20 - 3020 - 30Cured; ASTM D-2240
Tensile Strength 4.24 MPa615 psiCured; ASTM D-638
Elongation at Break 525 %525 %Cured; ASTM D-638
Tear Strength 27.2 kN/m155 pliCured; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 960 - 1440 min16.0 - 24.0 hourDemold
Working Life 50.0 - 85.0 min50.0 - 85.0 min
 
Descriptive Properties
AspectBlueCure
ColorBlueActivator
 WhiteSilicone
Mix Ratio100:10Silicone, Weight
 100:11Activator, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF194 / 317794

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.