MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M AC-350 Class B-4 Aerospace Sealant
Categories: Polymer; Thermoset; Polysulfide Sealant/Adhesive

Material Notes: 3M Aerospace Sealant AC-350 Class B are fast-cure, intermediate density polysulfide sealant suitable fro fuel tank and fuselage applications. These two-component, manganese dioxide cured sealant are solvent free and have resistance to aviation gasoline and jet fuel, as well as resistance to chemicals and petroleum products common to the aircraft industry. 3M AC-350 Class B Sealants maintain flexibility and bond strength on most metal substrates such as aluminum, titanium, steel, stainless steel, glass, and many coatings under extremes of temperature, weathering and stress. The mixed compound is a thixotropic paste easily applied by extrusion, injection gun or spatula, and exhibits good tooling properties.

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density <= 1.40 g/cc<= 0.0506 lb/in³cured 14 days @ 50% RH
Volatiles 2.0 %2.0 %
Brookfield Viscosity 900000 - 1.20e+6 cP900000 - 1.20e+6 cPBase, RVF #7 sp @ 2 rpm
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 50 - 5550 - 55cured 14 days @ 50% RH
Tensile Strength at Break 1.51 MPa219 psiStandard Heat cycle + JRF-12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C + 24 hrs at 49°C
 1.65 MPa239 psi24 hrs @ 121°C, and JRF-7 days @ 60°C
 1.79 MPa260 psiStandard Cure-14 days
 1.38 MPa
@Temperature 60.0 °C
200 psi
@Temperature 140 °F
JRF-14 days
 2.28 MPa
@Treatment Temp. 182 °C,
Time 28800 sec
331 psi
@Treatment Temp. 360 °F,
Time 8.00 hour
 2.55 MPa
@Treatment Temp. 121 °C,
Time 605000 sec
370 psi
@Treatment Temp. 250 °F,
Time 168 hour
Elongation at Break 42 %42 %Standard Heat cycle + JRF-12 days @ 60°C, 60 hrs @ 71°C, 6 hrs @ 82°C + 24 hrs at 49°C
 260 %260 %24 hrs @ 121°C, and JRF-7 days @ 60°C
 500 %500 %Standard Cure-14 days
 540 %
@Temperature 60.0 °C
540 %
@Temperature 140 °F
JRF-14 days
 100 %
@Treatment Temp. 182 °C,
Time 28800 sec
100 %
@Treatment Temp. 360 °F,
Time 8.00 hour
 125 %
@Treatment Temp. 121 °C,
Time 605000 sec
125 %
@Treatment Temp. 250 °F,
Time 168 hour
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °Fcured 14 days @ 50% RH
 182 °C360 °FShort term, cured 14 days @ 50% RH
Minimum Service Temperature, Air -54.0 °C-65.2 °Fcured 14 days @ 50% RH
 
Processing PropertiesMetricEnglishComments
Cure Time 1920 - 2160 min32.0 - 36.0 hour
Tack-Free Time 1920 - 2160 min32.0 - 36.0 hour
Shelf Life 9.00 Month
@Temperature <=26.7 °C
9.00 Month
@Temperature <=80.1 °F
 
Descriptive Properties
AppearanceBrownAccelerator
 Dark Gray
 Off WhiteBase

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMM35387 / 170134

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.