MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTAMID® HTplus M3036 PA10T/X, GF60  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA)

Material Notes: Characterization: 60% glass fibers, medium viscosity, stabilized; wide processing window; “green”, colors: natural, black

Applications: Dimension-stable, highly rigid technical parts for the use at high service temperatures and in contact with chemicals in automotives, electronics and machinery, metal replacement

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.71 g/ccISO 1183
Moisture Absorption 0.060 %50% RH; ISO 62
Water Absorption at Saturation 1.2 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 230 MPaISO 527-1/2
Elongation at Break 1.9 %ISO 527-1/2
Tensile Modulus 20100 MPaISO 527-1
Charpy Impact Unnotched 88.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 90.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 18.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 19.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+13 ohm-cmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µin/in-°F
@Temperature 23.0 - 55.0 °C
IOS 11359
Melting Point 285 °CISO 11357
Deflection Temperature at 0.46 MPa (66 psi) 288 °CISO 75-1
Deflection Temperature at 1.8 MPa (264 psi) 276 °CISO 75-1
Vicat Softening Point 292 °C
@Load 1.02 kg
Method A; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
IEC 60695
 HB
@Thickness 3.20 mm
IEC 60695

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Evonik Vestamid® L2140 Nylon 12
Evonik VESTAMID® HTplus C2505 PA10T/X
Kuraray Genestar™ G1301A-M61 Nylon, 30% Glass Filled
Kuraray Genestar™ G1300A-M41 Nylon, 30% Glass Filled
Evonik VESTAMID® NRG 6001 PA 12

PEVONIL253 / 196457

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.