MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Leaded Yellow Brass, UNS C85700, Copper Casting Alloy, Sand and Centrifugal Castings
Categories: Metal; Nonferrous Metal; Copper Alloy; Copper Casting Alloy

Material Notes:

Casting methods recommended for this alloy: Centrifugal, Investment, Plaster, and Sand.

Applications: Bushings, hardware fittings, ornamental castings.

Classified under: Yellow brasses and leaded yellow brasses. ASTM B584; formerly ASTM B146-6C

Typical data for sand castings or centrifugal castings, separately cast test bars. Alloy does not respond to heat treating

Key Words: Leaded naval brass, leaded yellow brass, 63-1-1-35, CA 857, ASTM B30 (CA857), ASTM B271, ASTM B584; ASTM B146-6C, SAE J462, Ingot code no. 406, FED QQ-C-390, MIL-C-15345 (Alloy 3)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.41 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 75
Tensile Strength, Ultimate 345 MPa
Tensile Strength, Yield 125 MPa
@Strain 0.5 %
Elongation at Break 40 %in 50 mm
Modulus of Elasticity 97.0 GPa
Machinability 80 %UNS C36000 (free-cutting brass) = 100%
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000078368 ohm-cm
@Temperature 20.0 °C
22% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
CTE, linear 22.0 µm/m-°C
@Temperature 20.0 - 260 °C
Specific Heat Capacity 0.376 J/g-°C
Thermal Conductivity 83.9 W/m-K
@Temperature 20.0 °C
Melting Point 903 - 920 °C
Solidus 903 °C
Liquidus 920 °C
Shrinkage 1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.55 %
Copper, Cu 58 - 64 %
Iron, Fe <= 0.70 %
Lead, Pb 0.80 - 1.5 %
Nickel, Ni <= 1.0 %
Silicon, Si <= 0.050 %
Tin, Sn 0.50 - 1.5 %
Zinc, Zn 32 - 40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Leaded Yellow Brass, UNS C85200, Copper Casting Alloy
Leaded Yellow Brass, UNS C85400, Copper Casting Alloy
Leaded Red Brass, UNS C83600, Copper Casting Alloy (Bronze SAE 40)
Leaded Yellow Brass, UNS C85800, Copper Casting Alloy, Die Castings
Leaded Semi-Red Brass, UNS C84800, Copper Casting Alloy

MC85700b1 / 11910

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.