MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

ExxonMobil Escorene® LD-723 High EVA Extrusion Coating Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: Data provided by the manufacturer, Exxon Chemical.

A high vinyl acetate extrusion coating resin which provides outstanding heat sealability and high clarity. It has a good balance of drawability and neck-in and can be coextruded with homopolymer extrusion coating resins on most coextrusion coating lines.

Applications: Heat seal layer for cheese packaging; Other extrusion coating applications requiring outstanding heat sealability.

Key Words: Ethylene Vinyl Acetate; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.940 g/cc0.0340 lb/in³Exxon Method
Environmental Stress Crack Resistance >= 500 hour>= 500 hourF50, Condition A; ASTM D1693
Melt Flow 22.5 g/10 min22.5 g/10 minExxon Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7777ASTM D2240
Hardness, Shore D 2727ASTM D2240
Tensile Strength, Ultimate 7.60 MPa1100 psiASTM D638
Elongation at Break >= 800 %>= 800 %ASTM D638
Flexural Modulus, 1% Secant 46.0 MPa6670 psiASTM D790
Tensile Impact Strength 282 kJ/m²134 ft-lb/in²23°C; ASTM D-1822
 
Thermal PropertiesMetricEnglishComments
Melting Point 85.0 °C185 °FExxon Method
Vicat Softening Point 55.0 °C131 °F1000g; ASTM D-1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® GP-22 ABS
Dow LDPE 640I Low Density Polyethylene, Liner Film Grade
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded

PEXCDU / 37870

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.