2-mil white, vinyl film; Specifically formulated for use on stainless steel; Pressure-activated adhesive for easy sliding, tacking, snap-up and repositioning; Flexible, conforms to moderate curves, corrugations and rivets; Permanent filmInformation provided by 3M |