MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Formosa Plastics Formolene® 2706N Impact Copolymer Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes: Copolymer for Heavy Duty Injection Molded Applications

Formolene® 2706N is a copolymer of polypropylene designed and formulated for injection molding applications. It contains a unique combination of stabilizers, nucleators and antistats, which give it an excellent balance of stiffness and impact strength. Formolene 2706N offers advantages in both processing and physical properties for applications including pails, crates and other Material Handling.

Formolene® 2706N complies with the U. S. Food and Drug Administration regulation 21 CFR 177.1520(c)(3.4). This material may only be used in contact with foods of type I, II, III, IV-B, VI, VII, VIII and IX as described in Table 1 of 21 CFR 176.170(c)

Specimens were injection molded according to the conditions specified in ASTM D4101

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 7.0 g/10 min
@Temperature 230 °C
7.0 g/10 min
@Temperature 446 °F
I2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 100100ASTM D785
Tensile Strength, Yield 18.6 MPa2700 psi2" (50mm) per min; ASTM D638
Elongation at Yield 7.0 %7.0 %2" (50mm) per min; ASTM D638
Flexural Modulus, 1% Secant 862 MPa125000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched  1.39 J/cm
@Temperature -30.0 °C
2.60 ft-lb/in
@Temperature -22.0 °F
ASTM D256
 1.60 J/cm
@Temperature -18.0 °C
3.00 ft-lb/in
@Temperature -0.400 °F
ASTM D256
 7.26 J/cm
@Temperature 0.000 °C
13.6 ft-lb/in
@Temperature 32.0 °F
ASTM D256
 7.47 J/cm
@Temperature 23.0 °C
14.0 ft-lb/in
@Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °C185 °FASTM D648
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene
Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene
Formosa Plastics Formolene® 5100J Blown and Cast Film Polypropylene
Flint Hills 44S2A Polypropylene Impact Copolymer
Formosa Plastics Formolene® 1102K Cast and BOPP Film Polypropylene

PFPCPQ018 / 150250

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.