MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Saint-Gobain CHR® TV350 Skived PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: CHR® T Series is manufactured from skived PTFE film coated with high-temperature silicone adhesive.

Features/Benefits: One side of T, TH, TV and TV350 have a silicone pressure sensitive adhesive and the other side offers low coefficient to friction PTFE film, which is thin and conformable. PTFE backing offers excellent high temperature resistance and is chemically inert. T, TH, TV and TV350’s tape construction is weather resistant, stable and non-toxic. T can be ordered to meet the requirements of MIL-I-23594C Type 1, Class 2; TV—Type 1, Class 4; TV320 – Type 1, Class 1.

Applications: T, TH, TV and TV350 are often used as an excellent release surface on packaging equipment and heat-sealing machines, roll coverings on plastic extruders, guide rails, and angle bars in the graphic arts industry.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 250 %
Tear Strength 15.0 pliInitial Tear Strength
Peel Strength 0.270 kN/mAdhesion to Steel
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 2230 V/mil
Dielectric Breakdown 7800 V
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 500 °F
Minimum Service Temperature, Air -100 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Saint-Gobain CHR® HM430 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® HM426 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® HM350 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
NuSil R33-2186 Silicone Two Part Sealing & Adhesive
NuSil GEL-8150 Silicone Gel

PSTGQZ347 / 68861

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.