MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Covestro Arcol® PPG-4000 Propylene Oxide
Categories: Polymer; Thermoset

Material Notes: Characterization: Arcol PPG-4000 polyol is a 4,000-molecular-weight diol based on propylene oxide.

Properties / Applications: Arcol PPG-4000 polyol is a high-performance, low-monol polyether that is prepared with Bayer ’s proprietary IMPACT® technology, using a patented organo-metallic propoxylation catalyst. The terminal end-groups are predominantly secondary hydroxyls and have a relatively low reactivity. This polyol is acidified with a low level of phosphoric acid, making it suitable for use in isocyanate-terminated prepolymers. Arcol PPG-4000 polyol is used in polyurethane and other applications, including cast elastomers, sealants, epoxy flexibilizers, defoamers, lubricants, crude oil de-emulsifiers and plasticizers. Arcol PPG-4000 polyol is a complementary product to Acclaim 6300 polyol, an ultra-low monol triol with the same equivalent weight. Overall polyol functionality can easily be varied by blending these two polyols. This polyol contains extremely low levels of monol. In some polyurethane systems, formulation changes, such as reducing the crosslinking level or changing the hard-segment content, may be necessary to maximize the benefits of using Acclaim polyols. As with any product, use of Arcol PPG-4000 polyol in a given application must be tested (including but not limited to field testing) in advance by the user to determine suitability.

Information provided by Covestro

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.01 g/cc1.01 g/cc
 0.940 g/cc
@Temperature 100 °C
0.940 g/cc
@Temperature 212 °F
 0.980 g/cc
@Temperature 50.0 °C
0.980 g/cc
@Temperature 122 °F
 1.02 g/cc
@Temperature 0.000 °C
1.02 g/cc
@Temperature 32.0 °F
Bulk Density 1.01 g/cc0.0363 lb/in³
Viscosity 980 cP980 cP
 100 cP
@Temperature 80.0 °C
100 cP
@Temperature 176 °F
 200 cP
@Temperature 60.0 °C
200 cP
@Temperature 140 °F
Storage Temperature 20.0 - 60.0 °C68.0 - 140 °F
 
Chemical PropertiesMetricEnglishComments
Acid Value <= 0.020<= 0.020[mg KOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point 213 °C415 °FPMCC
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.030 %<= 0.030 %
 
Descriptive Properties
AppearanceClear, viscous liquid
Color<50 Pt-Co
Hydroxyl number26.5-29.5 mg KOH/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Arcol® LHT-42 Polyether Polyol
Covestro Arcol® LG-650 Polyether Polyol
Covestro Arcol® PPG-425 Polypropylene Glycol
Covestro Arcol® PPG-1000 Polypropylene Glycol
Covestro Arcol® LHT-240 Polyether Polyol

PCOVEST0037 / 201820

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.