MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

PoolKemie KEMIEPOX NCT 301+ EH301 Pourable transparent Epoxy Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Introduction: Two-component epoxy product with high transparency, good chemical and dimensional stability and good mechanical resistance.

Application: Can be used to encapsulate electric circuits and incorporate artistic objects. Moreover can be used as adhesive in cement components and in formation of self leveling epoxy flooring, as well as in production of artistic and industrial manufactured articles.

Information provided by Poolkemie

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.05 - 1.15 g/cc1.05 - 1.15 g/ccA + B
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8282ASTM D 2240
Tensile Strength 50.0 MPa7250 psiASTM D 638
Elongation at Break 2.0 %2.0 %ASTM D 638
Flexural Strength 30.5 MPa4420 psiUNI 7219
Compressive Strength 85.0 MPa12300 psiASTM D 695
Compressive Modulus 2.30 GPa334 ksiASTM D 695
 
Processing PropertiesMetricEnglishComments
Cure Time 40.2 min0.670 hourPartial hardening
 1440 min24.0 hourComplete hardening
Pot Life 40.0 min40.0 minA + B
 
Descriptive Properties
Mixing ratio100+50A + B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPOOLK053 / 318532

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.