MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Konson DPTT-70 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 70% dipentamethylene thiuram tetrasulphide, 30% EPDM/EVA binder and dispersing agents

Use Characteristics: The curing accelerator Konson®DPTT-70 causes a very rapid and scorch-safe vulcanization of natural and sythetic rubbers. In combination with mercapto and sulphenamide accelerators, Konson® DPTT-70 is used as an activator and secon- dary accelerator. Konson®DPTT-70 is also used, in small amounts, in combination with other thiuram accelerators. The vulcanizates are then characterized by exceptionally good resistance to ageing. Konson® DPTT-70 is normally used for NR, SBR, NBR, IIR, BR, Hypalon etc.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion during the rubber mixing. Therefore, optimal activity of the effective DPTT is assured

Dosage levels: 0.35 - 3.5 phr for heat aging resistance rubber articles of all kinds.

Applications: It can be used as sulfurless curing agent, and it produces heat aging resistance rubber articles of all kinds, e.g. hoses, seals, bushing, especially based on EPDM and IIR. When used with Konson®MBTS-80, it can be used as accelerator for Hypalon rubber.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.25 g/cc
Ash <= 0.50 %
Evaporation Loss <= 0.30 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 105 °C
 
Descriptive Properties
AppearanceWhite to yellowish granules
Content= 96%DPTT
Sieve residue= 0.5 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKONS017 / 256062

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.