MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

CEN® Electronic Material CS Polyimide Tape
Categories: Polymer; Film; Thermoset; Polyimide, TS; Polyimide, Thermoset Film

Material Notes: CEN® CS polyimide tape is made of CEN® CN polyimide film coated with a high performance silicone adhesive. The tape shows excellent dielectric and insulation properties, high heat resistant, excellent solvent resistant, outstanding tear and abrasion resistance at elevated temperatures, and mask-off gold finger contacts during wave soldering.

Applications:

  1. Application in surface mounting process
    • PCB gold finger shielding
    • SMT wave soldering refluence soldering
    • Flexibility printed circuit fixed to the base board in SMT process
  2. Insulation in electrical equipments
    • Electronic high-tension transformer(Inverter)
    • F/H class electrical motor,transformers insulation binding
    • Lithium battery battery-pile insulation binding
  3. High temperature powder coating,electrostatic spraying masking
    • Electroplating protection
  4. Coil material splicing under high temperature

All information provided by CEN Electronic Material Co., LTD.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.0 microns0.984 milSubstrate; Standard
 25.0 microns0.984 milSubstrate; Testing Results
 60.0 microns2.36 milTotal; Standards
 63.0 microns2.48 milTotal; Testing Results
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield >= 73.3 MPa>= 10600 psi110 N/25mm; Standards
 >= 86.7 MPa>= 12600 psi130 N/25mm; Testing Results
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 1.00e+12 ohm1.00e+12 ohmStandards
 2.00e+12 ohm2.00e+12 ohmTesting Results
Dielectric Breakdown 5000 V5000 VStandards
 5200 V5200 VTesting Results
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 250 °C482 °F10 minutes; Pass
 
Descriptive Properties
Adhesion Strength (N/25mm)Standards
 Testing Results

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CEN® Electronic Material HT Polyimide Film
CEN® Electronic Material BL Polyimide Film
CEN® Electronic Material BX Polyimide Film
CEN® Electronic Material CV Polyimide Film, 2 Mil Thickness
Overview of materials for Polyimide, Thermoset Film

PCENE005 / 93467

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.