MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials Ketron™ LSG CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK); Polyetheretherketone, PEEK, Carbon Fiber Filled

Material Notes: Life Science Grade stock shapes, made from 30% carbon fiber-reinforced PEEK resin. Pre-assessed for biocompatibility on both resin and shape for up to 24 hours contact with body tissue according to USP VI and ISO 10993. Exhibits excellent mechanical strength, stiffness, resistance to chemicals and repeated sterilization via all current methods.

Vendors: TriStar Plastics Corp. provides engineering, custom fabrication and manufacturing of high-performance plastics and self-lubricating bearing materials, such as Rulon, PEEK, Torlon, CJ Composites and Ultracomp. Capabilities include component design, material selection, prototype and production, manufacturing and surface modification. Call (800) TRI-STAR (800) 874-7827 or visit or www.TStar.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.41 g/ccASTM D792
Water Absorption at Saturation 0.300 %ASTM D570 (17)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 102ASTM D785
Hardness, Shore D 90.0ISO 868
Tensile Strength 144 MPaISO 527-1/-2 (7)
Flexural Strength 220 MPaISO 178 (12)
Compressive Yield Strength 69.0 MPa
@Strain 1.00 %
ISO 604 (10)
 125 MPa
@Strain 2.00 %
ISO 604 (10)
 170 MPa
@Strain 5.00 %
ISO 604 (10)
Shear Strength 103 MPaASTM D732
Charpy Impact, Notched 5.00 kJ/m²ISO 179-1/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1e+05 - 1.00e+7 ohmANSI/ESD STM 11.11
Dielectric Strength 32.0 kV/inASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.0 µin/in-°FASTM E-831 (TMA)
 25.0 µm/m-°C
@Temperature 23.0 - 100 °C
 25.0 µm/m-°C
@Temperature 23.0 - 150 °C
 55.0 µm/m-°C
@Temperature >=150 °C
Thermal Conductivity 0.920 W/m-K
 6.40 BTU-in/hr-ft²-°F
Melting Point 644 °FASTM D3418
Maximum Service Temperature, Air 482 °FContinuous Use Temperature in Air after 20000 hr
Deflection Temperature at 1.8 MPa (264 psi) 518 °FASTM D648
Minimum Service Temperature, Air -20.0 °C
 
Compliance PropertiesOriginal ValueComments
USP Class VI Yes
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Continuous Sunlight Acceptable
Hot Water / Steam Acceptable
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Acceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Acceptable
 
Descriptive Properties
ESd categoryDissipative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials Ketron™ CA30 PEEK, Extruded 30% Carbon Fiber Reinforced Polyetherether Ketone
Overview of materials for Polyetheretherketone, Unreinforced
Mitsubishi Chemical Advanced Materials Ketron™ GF30 PEEK, Extruded 30% Glass-Reinforced Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ 1000 PEEK, Extruded Unfilled Polyetherether Ketone
Mitsubishi Chemical Advanced Materials Ketron™ CM CA30 PEEK Polyetheretherketone, 30% carbon fiber reinforced, compression molded

P1SM18J / 85176

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.