MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Braskem Green PE SHD7255LSL Injection Molding High Density Polyethylene  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Injection Molded

Material Notes: Description: SHC7260LS-L is a high-density polyethylene, developed for the injection molding which presents high hardness and stiffness, besides low tendency to warpage. This resin has additives against the ultraviolet radiation action. The minimum biobased content of this grade is 94%, determined according to ASTM D6866.

Application: Boxes for frozen food and agricultural products, industrial containers and boxes for general use, Safety Helmets, Toilet seats, Housewares, Toys, Lids, Caps &Closures, Pallets and Boxes for beverages bottles.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.954 g/ccASTM D792
ESCR 100% Igepal® <= 5.0 hour
@Temperature 50.0 °C
h/F50; Compression molded 2mm notched-plaques; ASTM D1693
Melt Flow 4.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 63ASTM D2240
Tensile Strength, Yield 27.0 MPaASTM D638
Flexural Modulus, 1% Secant 1270 MPaASTM D790
Izod Impact, Notched 45.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 74.0 °CASTM D648
Vicat Softening Point 127 °C10 N; ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Bamberger Polymers Bapolene® 3282 Injection Grade HDPE
Overview of materials for High Density Polyethylene (HDPE), Injection Molded
Braskem JV 060U HDPE Injection Molding Polyethylene
Braskem Green PE SHA7260 Injection Molding High Density Polyethylene
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene

PBRAS754 / 109540

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.