MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Ineos H07N-00 Polypropylene Homopolymer
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Grade H07N-00 is a barefoot polypropylene homopolymer with nucleation designed for extrusion processing. This resin meets the requirements of the U.S. Food and Drug administration as specified in 12 CFR 177.1520.
    Applications:
  • Cast film for hot-pack cheese applications
  • Flexible packaging
  • Cast films with higher stiffness requirements
    Benefits:
  • Processability
  • Barefoot additive package allows for customized packaging solutions with the addition of technical additives by the film manufacturer

Information provided by Ineos Olefins & Polymers USA

Key Words: With nucleation, designed for extrusion processing
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.904 g/cc0.0327 lb/in³ASTM D792
Melt Flow 7.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
7.3 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 107107ASTM D785
Tensile Strength at Break 20.0 MPa2900 psi2.0 in/min; ASTM D638
Tensile Strength, Yield 39.8 MPa5770 psi2.0 in/min; ASTM D638
Elongation at Break 31 %31 %2.0 in/min; ASTM D638
Elongation at Yield 6.5 %6.5 %2.0 in/min; ASTM D638
Flexural Modulus, 1% Secant 2100 MPa304000 psiASTM D790A
Izod Impact, Notched 0.262 J/cm0.490 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 2.58 kJ/m²1.23 ft-lb/in²Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 127 °C260 °FUnannealed; ASTM D648
 
Optical PropertiesMetricEnglishComments
Haze 38 %
@Thickness 1.27 mm
38 %
@Thickness 0.0500 in
ASTM D1003
Gloss 94 %94 %60°; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessCoating
 Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos H07B-01 Polypropylene Homopolymer
Ineos 3950 Polypropylene Impact Copolymer
Ineos H02C-00 Polypropylene Homopolymer
Ineos 3560 Polypropylene Impact Copolymer
Formosa Plastics Formolene® 5144L Homopolymer Polypropylene

PINEOS906 / 130365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.