MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos Mecoline I RDX 5233 Radiation cross-linkable polyalkene compound
Categories: Polymer; Thermoplastic

Material Notes: Radiation cross-linkable polyalkene compound

Compound class: Insulation

Compound category: RDX

Flame retardant: Not flame retardant

Standards: SAE AS-81044/9; SAE AS 81044/11; NEMA WC 27500; SAE AS-81044/12

Typical applications: This compound is an excellent choice for manufacturing insulated hook-up wires in military and aerospace industries (airframe wire) and component conductors for NEMA WC 275000 cables.

Features: Low smoke; Oil resistant; Abrasion resistant; High temperature resistant

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³pressed plaques; DIN EN ISO 1183-1A
Melt Flow 12 g/10 min
@Load 21.6 kg,
Temperature 190 °C
12 g/10 min
@Load 47.6 lb,
Temperature 374 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060pressed plaques; DIN ISO 7619-1
Tensile Strength >= 20.0 MPa>= 2900 psicross-linked plaques or tapes, 250kGy; IEC 60811-501
 >= 30.0 MPa>= 4350 psiextruded tapes; IEC 60811-501
Elongation at Break >= 400 %>= 400 %cross-linked plaques or tapes, 250kGy; IEC 60811-501
 >= 700 %>= 700 %extruded tapes; IEC 60811-501
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 180 °C338 - 356 °FTool
 180 °C356 °FMaximum mass temperature
Zone 1 140 - 150 °C284 - 302 °F
Zone 2 150 - 160 °C302 - 320 °F
Zone 3 160 - 170 °C320 - 338 °F
Zone 4 170 - 180 °C338 - 356 °F
Zone 5 170 - 180 °C338 - 356 °F
Adapter Temperature 170 - 180 °C338 - 356 °F
Head Temperature 170 - 180 °C338 - 356 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Shelf Life 12.0 Month12.0 Month

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS040 / 296147

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.