MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil EXACT™ 203 Plastomer for Polymer Modification  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Ethylene octene copolymer produced using ExxonMobil Chemical Exxpol technology, exhibiting both plastic and elastomeric properties. Designed for modification of both polypropylenes and polyethylenes in applications such as injection molding, cast film, and profile extrusion.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.902 g/ccExxonMobil Method
Mooney Viscosity 9.1
@Temperature 125 °C
ML (1 + 4); ASTM D1646
Melt Flow 3.0 g/10 minASTM D1238
 6.8 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 8715s; ASTM D2240
Hardness, Shore D 4215s; ASTM D2240
Tensile Stress at Strain 943 psi
@Strain 100 %
ASTM D412
 986 psi
@Strain 300 %
ASTM D412
Flexural Modulus, 1% Secant 11100 psiASTM D790
Izod Impact, Notched NBASTM D256
 NB
@Temperature -40.0 °C
ASTM D256
Instrumented Impact Total Energy 19.6 ft-lb
@Temperature 23.0 °C
ASTM D3763
 22.7 ft-lb
@Temperature -40.0 °C
ASTM D3763
Instrumented Impact Energy at Peak 12.8 ft-lb
@Temperature -40.0 °C
ASTM D3763
 14.4 ft-lb
@Temperature 23.0 °C
ASTM D3763
Tear Strength 75.1 kN/mDie C; ASTM D412
 
Thermal PropertiesOriginal ValueComments
Melting Point 201.4 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 200.3 °Fat 200g; ASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 88 %
@Thickness 1.27 mm
ASTM D1003
 
Descriptive Properties
FormPellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil EXACT™ 8210 Plastomer for Polymer Modification
ExxonMobil EXACT™ 3035 Plastomer for Polymer Modification
Trinseo Magnum™ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Trinseo EMERGE™ PC/PET 9100CR MED Polycarbonate Resin
ExxonMobil EXACT™ 230 Plastomer for Polymer Modification

PEXB359 / 37664

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.