MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

China Tungsten YG15 Tungsten Carbide for Dies and Wear Part Making
Categories: Ceramic; Carbide

Material Notes: For drawing of steel bars and pipes at high reduction; and also for upsetting, perforating and stamping tools under higher-stress conditions.

Information provided by China Tungsten

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 13.9 - 14.2 g/cc0.502 - 0.513 lb/inĀ³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell A >= 87>= 87
Flexural Strength 2060 MPa299000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
China Tungsten YG15 Tungsten Carbide Powder
China Tungsten YG15 Cemented Tungsten Carbide for Mining Purposes
Titanium Ti-6Al-4V (Grade 5), Annealed
Goodfellow Tungsten Carbide/Cobalt

NCHIN090 / 78932

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.