MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Kohesi Bond KB 1452 LV Two component, room temperature curing epoxy offering good flowability
Categories: Polymer; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced

Material Notes: Product Highlights:
  • High glass transition temperature
  • Resists multiple sterilization cycles
  • Castable up to 3 inches; ideal for potting
  • Superior chemical resistance
  • Exceptional electrical insulation properties
  • Superb flow properties
Kohesi Bond KB 1452 LV is a two component, room temperature curing, epoxy system suitable for bonding, sealing, potting and encapsulation. It has a favorable 100:40 (Part A: Part B) mix ratio by weight or 100:50 (Part A: Part B) mix ratio by volume. This epoxy system offers excellent adhesion to wide variety of substrates including metals, ceramics, most plastics and glass. It readily cures at room temperature and can achieve faster cures at elevated temperatures. The optimal cure schedule is an overnight room temperature set-up followed by a heat cure at 70°C - 90°C for 3 - 5 hours. KB 1452 LV offers an extensive service temperature range of -50°C to +200°C. This adhesive fosters outstanding physical strength properties as well as dimensional stability. It offers minimal shrinkage upon cure and is castable up to 3 inches depth. In addition to superior electrical insulation, it also offers excellent chemical resistance to a variety of fuels, oils and water. Part A is clear and Part B is amber in color. Once mixed it is amber clear in color. KB 1452 LV is widely used in the electronics, medical, optical, optoelectronic and specialty OEM applications.

Typical Applications:

  • Bonding
  • Sealing
  • Coating
  • Potting
  • Encapsulation

Information provided by Kohesi Bond Custom Engineered Adhesives

Vendors: Kohesi Bond is a pioneer in manufacturing over 300 grades of custom engineered adhesives, sealants, coatings, potting and encapsulation compounds. Our first-rate adhesives are tailor-fitted to meet your exact specifications and offer superior strength and performance in your application. Learn more about Kohesi Bond’s industry-ready products at kohesibond.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Viscosity 30 - 80 cP30 - 80 cPPart B
 10000 - 14000 cP10000 - 14000 cPPart A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 75>= 75
Tensile Strength >= 84.1 MPa>= 12200 psi
Tensile Modulus 2.48 - 2.76 GPa360 - 400 ksi
Adhesive Bond Strength >= 14.5 MPa>= 2100 psiTensile Lap Shear, Al/Al
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cm
Dielectric Constant 3.81
@Frequency 60 Hz
3.81
@Frequency 60 Hz
Dielectric Strength 17.3 kV/mm
@Thickness 3.17 mm
440 kV/in
@Thickness 0.125 in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 35.0 - 40.0 µm/m-°C19.4 - 22.2 µin/in-°F
Maximum Service Temperature, Air 200 °C392 °F
Minimum Service Temperature, Air -50.0 °C-58.0 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.63
@Wavelength 589 nm
1.63
@Wavelength 589 nm
 
Processing PropertiesMetricEnglishComments
Cure Time  120 - 180 min
@Temperature 90.0 °C
2.00 - 3.00 hour
@Temperature 194 °F
Option 2
 120 - 180 min
@Temperature 90.0 °C
2.00 - 3.00 hour
@Temperature 194 °F
Optimum Cure: Overnight at 23°C, followed by 2-3 hours at 90°C
 2880 - 4320 min
@Temperature 23.0 °C
48.0 - 72.0 hour
@Temperature 73.4 °F
Option 1
Working Life 35.0 - 75.0 min35.0 - 75.0 min100 g of mixed epoxy
Shelf Life 12.0 Month12.0 Monthin original unopened containers

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKOHESI950 / 249129

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.