Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 1.18 g/cc | 1.18 g/cc |
Density | 1.19 g/cc | 0.0430 lb/in³ |
Moisture Absorption | 0.0200 % | 0.0200 % |
| 0.150 % | 0.150 % |
Water Absorption at Saturation | 0.35 % | 0.35 % |
Viscosity | 9.0 cP @Load 1.20 kg, Temperature 300 °C | 9.0 cP @Load 2.65 lb, Temperature 572 °F |
Linear Mold Shrinkage, Flow | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0080 in/in @Thickness 0.126 in |
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0080 cm/cm @Thickness 3.20 mm | 0.0040 - 0.0080 in/in @Thickness 0.126 in |
Melt Flow | 10 g/10 min @Load 1.20 kg, Temperature 300 °C | 10 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Rockwell L | 89 | 89 |
Hardness, Rockwell R | 121 | 121 |
Tensile Strength at Break | 50.0 MPa | 7250 psi |
| 60.0 MPa | 8700 psi |
Tensile Strength, Yield | 55.0 MPa | 7980 psi |
| 57.0 MPa | 8270 psi |
Elongation at Break | 98 % | 98 % |
| 120 % | 120 % |
Elongation at Yield | 6.0 % | 6.0 % |
| 6.0 % | 6.0 % |
Tensile Modulus | 2.02 GPa | 293 ksi |
| 2.15 GPa | 312 ksi |
Flexural Strength | 85.0 MPa | 12300 psi |
| 92.0 MPa | 13300 psi |
Flexural Modulus | 2.23 GPa | 323 ksi |
| 2.25 GPa | 326 ksi |
Izod Impact Notched | 865 J | 638 ft-lb |
| 774 J @Temperature -30.0 °C | 571 ft-lb @Temperature -22.0 °F |
Izod Impact, Notched (ISO) | 70.0 kJ/m² | 33.3 ft-lb/in² |
| 60.0 kJ/m² @Temperature -30.0 °C | 28.6 ft-lb/in² @Temperature -22.0 °F |
Izod Impact, Unnotched (ISO) | NB | NB |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
Charpy Impact Unnotched | NB | NB |
| NB @Temperature -30.0 °C | NB @Temperature -22.0 °F |
Charpy Impact, Notched | 7.00 J/cm² | 33.3 ft-lb/in² |
| 6.50 J/cm² @Temperature -30.0 °C | 30.9 ft-lb/in² @Temperature -22.0 °F |
Dart Drop, Total Energy | 70.0 J | 51.6 ft-lb |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | >= 1.00e+15 ohm-cm | >= 1.00e+15 ohm-cm |
Surface Resistance | >= 1.00e+15 ohm | >= 1.00e+15 ohm |
Dielectric Constant | 2.64 @Frequency 1e+6 Hz | 2.64 @Frequency 1e+6 Hz |
| 2.68 @Frequency 100 Hz | 2.68 @Frequency 100 Hz |
Dielectric Strength | 16.2 kV/mm @Thickness 0.800 mm | 411 kV/in @Thickness 0.0315 in |
Dissipation Factor | 0.0012 @Frequency 100 Hz | 0.0012 @Frequency 100 Hz |
| 0.0093 @Frequency 1e+6 Hz | 0.0093 @Frequency 1e+6 Hz |
Hot Wire Ignition, HWI | >= 120 sec @Thickness >=0.700 mm | >= 120 sec @Thickness >=0.0276 in |
High Amp Arc Ignition, HAI | 60 - 120 arcs @Thickness >=0.700 mm | 60 - 120 arcs @Thickness >=0.0276 in |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear, Parallel to Flow | 70.0 µm/m-°C @Temperature -40.0 - 40.0 °C | 38.9 µin/in-°F @Temperature -40.0 - 104 °F |
| 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C | 40.0 µin/in-°F @Temperature 73.4 - 176 °F |
CTE, linear, Transverse to Flow | 72.0 µm/m-°C @Temperature 23.0 - 80.0 °C | 40.0 µin/in-°F @Temperature 73.4 - 176 °F |
| 74.7 µm/m-°C @Temperature -40.0 - 40.0 °C | 41.5 µin/in-°F @Temperature -40.0 - 104 °F |
Hot Ball Pressure Test | 125 °C | 257 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 140 °C | 284 °F |
| 139 °C @Thickness 3.20 mm | 282 °F @Thickness 0.126 in |
Deflection Temperature at 1.8 MPa (264 psi) | 128 °C | 262 °F |
| 124 °C @Thickness 3.20 mm | 255 °F @Thickness 0.126 in |
Vicat Softening Point | 145 °C | 293 °F |
| 145 °C | 293 °F |
| 146 °C | 295 °F |
UL RTI, Electrical | 130 °C | 266 °F |
UL RTI, Mechanical with Impact | 120 °C | 248 °F |
UL RTI, Mechanical without Impact | 130 °C | 266 °F |
Flammability, UL94 | HB @Thickness >=0.700 mm | HB @Thickness >=0.0276 in |
Oxygen Index | 37 % | 37 % |
Glow Wire Ignition Temperature | 875 °C @Thickness 0.800 mm | 1610 °F @Thickness 0.0315 in |
| 875 °C @Thickness 1.00 mm | 1610 °F @Thickness 0.0394 in |
| 875 °C @Thickness 1.50 mm | 1610 °F @Thickness 0.0591 in |
| 875 °C @Thickness 3.00 mm | 1610 °F @Thickness 0.118 in |
Glow Wire Flammability Index | 850 °C @Thickness 0.800 mm | 1560 °F @Thickness 0.0315 in |
| 960 °C @Thickness 1.00 mm | 1760 °F @Thickness 0.0394 in |
| 960 °C @Thickness 1.50 mm | 1760 °F @Thickness 0.0591 in |
| 960 °C @Thickness 3.00 mm | 1760 °F @Thickness 0.118 in |
|
Processing Properties | Metric | English | Comments |
---|
Nozzle Temperature | 290 - 310 °C | 554 - 590 °F |
Zone 2 | 280 - 305 °C | 536 - 581 °F |
Zone 3 | 295 - 315 °C | 563 - 599 °F |
Melt Temperature | 295 - 315 °C | 563 - 599 °F |
Mold Temperature | 70.0 - 95.0 °C | 158 - 203 °F |
Drying Temperature | 120 °C | 248 °F |
Dry Time | 3.00 - 4.00 hour | 3.00 - 4.00 hour |
| 48.0 hour | 48.0 hour |
Back Pressure | 0.300 - 0.700 MPa | 43.5 - 102 psi |
Shot Size | 40 - 60 % | 40 - 60 % |
Vent Depth | 0.00250 - 0.00760 cm | 0.000984 - 0.00299 in |
Screw Speed | 40 - 70 rpm | 40 - 70 rpm |
|
Descriptive Properties |
---|
UV-light, water exposure/immersion | F1 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding