MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Alathon® L4904 High Density Polyethylene, Pipe and Sheet Extrusion Grade
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Pipe Grade

Material Notes: Alathon L4904 is a bimodal, high molecular weight, high density polyethylene resin with excellent processability characteristics that meet the high performance requirements of demanding pressure pipe applications including gas distribution, industrial piping, gas gathering, municipal water service lines and sewers. L4904 is designed specifically to provide resistance to pipe failure by rapid crack propagation and slow crack growth mechanisms. When L4904 is compounded with an Equistar approved black at the correct loading (see page 2) this formula meets the following standards.
  • Plastics Pipe Institute (PPI) PE 4710.
  • PE 100 per PPI TR-4.
  • ASTM D 3350 Cell Classification 445574C and 445576C.
  • Chemical Resistance per ASTM D 2513
  • NSF Standard 14 and Standard 61 for Potable Water Pipe and Fittings.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D1505
Melt Flow 0.040 g/10 minASTM D1238
 7.0 g/10 minHigh Load; ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
PENT >= 2000 hour
@Temperature 80.0 °C
2.4MPa
Tensile Strength at Break 5100 psiASTM D638
Tensile Strength, Yield 3500 psiASTM D638
Elongation at Break 800 %ASTM D638
Creep Strength 12.4 MPa
@Temperature 20.0 °C,
Time >=720000 sec
2% Secant Modulus 146000 psiASTM D790
Hydrostatic Design Basis 1600 psiASTM D2837
 1000 psi
@Temperature 60.0 °C
ASTM D2837
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -76.0 °CASTM D746
DSC Induction Temperature 250 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borstar® FB3450 HDPE for Film Extrusion
LyondellBasell Alathon® L5008HP High Density Polyethylene, Pressure Pipe Extrusion Grade
Borealis Bormed™ HE2581-PH HDPE for Healthcare Applications
Chevron Phillips Marlex® HP076 High Density Polyethylene, Pipe Grade
Chevron Phillips Marlex® HP132 High Density Polyethylene, Pressure Pipe Grade

PEQU0800 / 104156

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.