MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sarlink® TPV X10060B Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X10060B is a high performance thermoplastic vulcanite used in automotive applications. This product is a low hardness, low density, RoHS compliant grade exhibiting superior compression set and chemical resistance. This grade is suitable for injection molding.

Availability: Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Color Stability; Good Processability; Heat Aging Resistance; Low Compression Set; Low Fogging; Medium Hardness; Low Specific Gravity; Lubricated; UV Resistant; Weather Resistant

Uses: Automotive Applications; Automotive Exterior Parts; Overmolding

RoHS Compliance: RoHS Compliant

Automotive Specifications: FORD WSD-M2D49-A2 Color: Black

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.902 g/cc0.0326 lb/in³ISO 1183
Viscosity 180 cP
@Shear Rate 206 1/s,
Temperature 200 °C
180 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Apparent; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  58
@Time 5.00 sec
58
@Time 0.00139 hour
Extruded; ISO 868
 61
@Time 5.00 sec
61
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 4.40 MPa638 psiAcross Flow; ISO 37
 4.40 MPa638 psiFlow; ISO 37
 3.34 MPa
@Treatment Temp. 135 °C,
Time 3.629e+6 sec
485 psi
@Treatment Temp. 275 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 3.39 MPa
@Treatment Temp. 150 °C,
Time 605000 sec
491 psi
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Tensile Stress at Strain  2.00 MPa
@Strain 100 %
290 psi
@Strain 100 %
Across Flow; ISO 37
 2.40 MPa
@Strain 100 %
348 psi
@Strain 100 %
Flow; ISO 37
 1.92 MPa
@Strain 100 %,
Treatment Temp. 135 °C
278 psi
@Strain 100 %,
Treatment Temp. 275 °F
Across Flow, Change in Air at 1008 hr; ISO 188
 1.94 MPa
@Strain 100 %,
Treatment Temp. 150 °C
281 psi
@Strain 100 %,
Treatment Temp. 302 °F
Across Flow, Change in Air at 168 hr; ISO 188
Elongation at Break 300 %300 %Flow; ISO 37
 370 %370 %Across Flow; ISO 37
 289 %
@Treatment Temp. 135 °C,
Time 3.629e+6 sec
289 %
@Treatment Temp. 275 °F,
Time 1008 hour
Across Flow, Change in Air; ISO 188
 292 %
@Treatment Temp. 150 °C,
Time 605000 sec
292 %
@Treatment Temp. 302 °F,
Time 168 hour
Across Flow, Change in Air; ISO 188
Coefficient of Friction 0.50 - 0.600.50 - 0.60ISO 1183
Tear Strength 16.0 kN/m91.0 pliMethod Ba, Angle (Unnicked), Across Flow; ISO 34-1
Compression Set  18 %
@Temperature 22.8 °C,
Time 79200 sec
18 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 27 %
@Temperature 70.0 °C,
Time 79200 sec
27 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 45 %
@Temperature 125 °C,
Time 252000 sec
45 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 180 - 205 °C356 - 401 °F
Middle Barrel Temperature 180 - 205 °C356 - 401 °F
Front Barrel Temperature 180 - 205 °C356 - 401 °F
Nozzle Temperature 180 - 205 °C356 - 401 °F
Melt Temperature 180 - 205 °C356 - 401 °F
Mold Temperature 10.0 - 55.0 °C50.0 - 131 °F
Screw Speed 100 - 200 rpm100 - 200 rpm
 
Descriptive Properties
AppearanceBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teknor Apex Chemlon 100 X Nylon 66, Lubricated GP

PTEKNQ1225 / 237716

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.