Applications include cold drawn or finished bar, cold punched nuts, split rivets, machine screws, and wood screws. Post oil quenched hardness: 30 HRC surface, 27 HRC half-radius, 22 HRC center. |
UNS G11440, ASTM A29, ASTM A108, ASTM A311, FED QQ-S-637 (C1144), SAE J403, SAE J412, SAE J414 |