MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Chemical Concepts Chem-Set™ 205M Contact bond adhesive
Categories: Polymer; Adhesive; Thermoset

Material Notes: Chem-set™ AW 205 is a high performance contact bond adhesive in a non-flammable solvent. Chem-set™ AW 205 is suitable for bonding decorative laminate, wood, particleboard, metal, rubber, hardboard, plywood, leather, canvas and many other materials. It is fast drying, oil and waterproof and requires no clamping. Its high tack plus excellent combinability and green strength provides uniform high strength bonds under a wide variety of laminating condition.

FEATURES: Quick Dry Time High Strength Bonds, Aggressive Grab Tack Good Spray Pattern, High Green Strength, Post formable, Excellent adhesion to many substrates, Long Open Time.

Information provided by Chemical Concepts™.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 15 %15 %+-1.5%
Volatile Organic Compounds (VOC) Content 71.4 g/l71.4 g/lEPA Method 24
Viscosity 325 - 425 cP325 - 425 cP
 
Processing PropertiesMetricEnglishComments
Shelf Life 9.00 Month9.00 MonthFrom date of manufacture, unopened container, stored @ 60°F-80°F.
 
Descriptive Properties
Air Dry Time2 to 5 minutes
Chemical CompositionCompound Neoprene & Methylene Chloride solvent
Colorclear/green
Open Time60 minutes
Weight10.74

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHEMI911 / 232227

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.