System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Eneos N230SV Nitrile Rubber
Categories:
Polymer
;
Thermoset
;
Rubber or Thermoset Elastomer (TSE)
Material Notes:
Characteristics: Low Mooney type N230SL,High cold flow
Application: Various packings, gaskets, hoses, PVC blends, adhesives
ENEOS has acquired the elastomer product lines from JSR Corporation.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Specific Gravity
0.980
g/cc
0.980
g/cc
Mooney Viscosity
32
@Temperature 100 °C
32
@Temperature 212 °F
ML1+4
40
@Temperature 100 °C
40
@Temperature 212 °F
ML1+4, Compound (non-vulcanized)
20
@Temperature 125 °C,
Time 64800 sec
20
@Temperature 257 °F,
Time 18.0 hour
Scorch Test, ML1, Compound (non-vulcanized)
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
68
68
68
68
Compound (vulcanized)
55
@Temperature 40.0 °C,
Time 173000 sec
55
@Temperature 104 °F,
Time 48.0 hour
Fuel Oil B, Compound (non-vulcanized)
56
@Temperature 120 °C,
Time 252000 sec
56
@Temperature 248 °F,
Time 70.0 hour
IRM903, Compound (vulcanized)
64
@Temperature 120 °C,
Time 252000 sec
64
@Temperature 248 °F,
Time 70.0 hour
Air heat Aging, Compound (non-vulcanized)
67
@Temperature 120 °C,
Time 252000 sec
67
@Temperature 248 °F,
Time 70.0 hour
IRM901, Compound (vulcanized)
Tensile Strength
18.0
MPa
2610
psi
18.0
MPa
2610
psi
Compound (vulcanized)
8.28
MPa
@Temperature 40.0 °C,
Time 173000 sec
1200
psi
@Temperature 104 °F,
Time 48.0 hour
Fuel Oil B, Compound (non-vulcanized)
16.38
MPa
@Temperature 120 °C,
Time 252000 sec
2376
psi
@Temperature 248 °F,
Time 70.0 hour
IRM903, Compound (vulcanized)
18.9
MPa
@Temperature 120 °C,
Time 252000 sec
2740
psi
@Temperature 248 °F,
Time 70.0 hour
IRM901, Compound (vulcanized)
19.08
MPa
@Temperature 120 °C,
Time 252000 sec
2767
psi
@Temperature 248 °F,
Time 70.0 hour
Air heat Aging, Compound (non-vulcanized)
Elongation at Break
480 %
480 %
480 %
480 %
Compound (vulcanized)
249.6 %
@Temperature 40.0 °C,
Time 173000 sec
249.6 %
@Temperature 104 °F,
Time 48.0 hour
Fuel Oil B, Compound (non-vulcanized)
321.6 %
@Temperature 120 °C,
Time 252000 sec
321.6 %
@Temperature 248 °F,
Time 70.0 hour
Air heat Aging, Compound (non-vulcanized)
355.2 %
@Temperature 120 °C,
Time 252000 sec
355.2 %
@Temperature 248 °F,
Time 70.0 hour
IRM901, Compound (vulcanized)
408 %
@Temperature 120 °C,
Time 252000 sec
408 %
@Temperature 248 °F,
Time 70.0 hour
IRM903, Compound (vulcanized)
100% Modulus
2.60
MPa
377
psi
Compound (vulcanized)
300% Modulus
12.4
MPa
1800
psi
12.4
MPa
1800
psi
Compound (vulcanized)
Resilience
33
33
[%], Rebound, Compound (vulcanized)
Tear Strength
47.0
kN/m
268
pli
Compound (vulcanized)
Compression Set
14 %
@Temperature 100 °C,
Time 252000 sec
14 %
@Temperature 212 °F,
Time 70.0 hour
Compound (vulcanized)
19 %
@Temperature 120 °C,
Time 252000 sec
19 %
@Temperature 248 °F,
Time 70.0 hour
Compound (vulcanized)
Thermal Properties
Metric
English
Comments
Brittleness Temperature
-29.0
°C
-20.2
°F
Descriptive Properties
Acrylonitrile Content (%)
35
Delta;V
100
(%)
0
IRM901 70 hrs at 120°C, Compound (vulcanized)
19
IRM903 70 hrs at 120°C, Compound (vulcanized)
2
Distilled Water 70 hr at 40°C, Compound (non-vulcanized)
270
Fuel Oil B 48 hrs at 40°C, Compound (non-vulcanized)
47
Fuel Oil C 48 hrs at 40°C, Compound (non-vulcanized)
80
Fuel Oil C/Ethanol 48 hrs at 40°C, Compound (non-vulcanized)
Extrusion Test
420 cc/min
80°C, 25 rpm, Extrusion Volume
455 cm/min
80°C, 25 rpm, Extrusion Length
60
80°C, 25 rpm, Die Swell %
Flex Test
11
Growth 2 to 15 mm (Thousand Times)
Flow Rate
96
Q×10
4
, 80°C, 100 kg, Kokahiki Flow tester
JSR Mold Curast Test 160°C, Minutes
2
t
c(10)
5
t
c(90)
Low-Temperature Torsion Test
-24°C
t10
-30°C
t100
Mill Contraction 50°C (%)
45
Ozone Degradability Test
C-3
Static 20% Elongation, 50 ppm 5 Hours at 40°C
C-3
Dynamic 0 to 20% Elongation, 50 ppm 5 Hours at 40°C
Product form
Bale
Product Stain
NS
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PJSRC8063 / 295379
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.