MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Free-cutting phosphor bronze, UNS C54400, H04 Temper 19 mm flat products
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze

Material Notes: Good to excellent corrosion resistance. Excellent machinability, good cold workability. Fabricated by blanking, drawing, bending, machining, shearing, stamping.

Applications: bearings, bushings, gears, pinions, shafts, thrust washers, valve parts.

Test specimen: flat products - 19mm thickness.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 380 MPa
@Thickness 19.0 mm
55100 psi
@Thickness 0.748 in
Flat products
Tensile Strength, Yield 240 MPa
@Strain 0.5 %,
Thickness 19.0 mm
34800 psi
@Strain 0.5 %,
Thickness 0.748 in
Flat products
Elongation at Break 25 %
@Thickness 19.0 mm
25 %
@Thickness 0.748 in
in 50 mm, Flat products
Modulus of Elasticity 103 GPa14900 ksi
Poissons Ratio 0.3210.321
Machinability 80 %80 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa5660 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000910 ohm-cm
@Temperature 20.0 °C
0.00000910 ohm-cm
@Temperature 68.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.3 µm/m-°C
@Temperature 20.0 - 300 °C
9.61 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.380 J/g-°C0.0908 BTU/lb-°F
Thermal Conductivity 87.0 W/m-K
@Temperature 20.0 °C
604 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 930 - 1000 °C1710 - 1830 °F
Solidus 930 °C1710 °F
Liquidus 1000 °C1830 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 88 %88 %
Iron, Fe <= 0.10 %<= 0.10 %
Lead, Pb 3.5 - 4.5 %3.5 - 4.5 %
Phosphorus, P 0.010 - 0.50 %0.010 - 0.50 %
Tin, Sn 3.5 - 4.5 %3.5 - 4.5 %
Zinc, Zn 1.5 - 4.5 %1.5 - 4.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Free-cutting phosphor bronze, UNS C54400, H10 Temper sheet/strip
Free-cutting phosphor bronze, UNS C54400, H04 Temper sheet/strip
Free-cutting phosphor bronze, UNS C54400, H02 Temper sheet/strip
Free-cutting phosphor bronze, UNS C54400
Free-cutting phosphor bronze, UNS C54400, H04 Temper 8 mm flat products

MC54400c3 / 11571

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.