MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials GE Silicones UltraGlaze SSG4400A + SSG4400B Structural Silicone Glazing Adhesive
Categories: Polymer; Adhesive; Thermoset; Silicone

Material Notes: GE SSG4400 UltraGlaze is a high-modulus neutral curing structural silicone elastomeric adhesive for use in shop, factory and field glazing of curtain wall panels. SSG4400 is a two-component product (part A + part B) that upon mixing, yields rapid and thorough deep-section cure, fast durometer and strength build and quick curing to high strength durable silicone rubber. Performance: Silicone durability, Primerless adhesion, Low pumping viscosity, Fast durometer & strength build. Application: SSG4400 is suitable for use in structural glazing applications such as factory or field glazing of curtain wall units and modules for unitized and panelized systems. SSG4400 is suitable for use as a weather seal product, when movement expected in the joint does not exceed its movement capability (±25%).

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc1.03 g/ccSSG4400B
 1.37 g/cc1.37 g/cc
 1.42 g/cc1.42 g/ccSSG4400A
Volatile Organic Compounds (VOC) Content 27 g/l27 g/l
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 35 - 4035 - 40ASTM D2240
Tensile Strength 1.00 MPa
@Thickness 6.35 mm
145 psi
@Thickness 0.250 in
ASTM C1135
Elongation, Ultimate 102 %
@Thickness 6.35 mm
102 %
@Thickness 0.250 in
ASTM C1135
Shear Strength 1.06 MPa154 psiASTM C961
Tear Strength 6.84 kN/m39.0 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 149 °C300 °FHeat Resistance
 
Processing PropertiesMetricEnglishComments
Shelf Life 12.0 Month12.0 MonthSSG4400B. When stored properly.
 18.0 Month18.0 MonthSSG4400A. When properly stored.
 
Descriptive Properties
AppearanceThixotropic PasteMixed
 Thixotropic PasteUncured. SSG4400A.
 Thixotropic PasteUncured. SSG4400B.
ColorBlackCured
 BlackSSG4400A + SSG4400B
 BlackSSG4400A+SSG4400B mixed
 BlackUncured. SSG4400B.
 WhiteUncured. SSG4400A.
Consistency / Sag0.1"Non-sagging
Cyclic Movement Capacity+/- 25%ASTM C719
Mix Ratio12:1 by weightAs Tested
 9:1 to 14:1By weight
Snap Time15-75 minutes
Tooling Time15 + minutes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9915 / 265724

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.