MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Riken Technos RIKEBIO® RB-LI70C1 TPE
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Product: Compound

Plastic Type: Elastomer

Field or Business Category: Daily Life & Healthcare/Life & Industrial Materials

Parts: Life & Industrial Materials

Special Features: RB-LI70C1 is an environmentally friendly thermoplastic elastomer compound using plant-derive draw. It can be handled with the same molding machine as a general TPE compound. Excellent transparency. The biomass content of it is 32%, which can contribute to the reduction of environmental impact, which is becoming more socially demanding.

Information provided by Riken Technos Corp.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccJIS K 7112
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 71
@Time 15.0 sec
71
@Time 0.00417 hour
JIS K 6253
Tensile Strength 9.00 MPa1310 psiJIS K 6251
Elongation at Break 550 %550 %JIS K 6251

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRIKEN053 / 314268

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.