MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Chromium-Bearing Copper-Nickel, UNS C71900, Spring Temper
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Applications: Heat exchanger tubes, tube sheets, water boxes, ferrules, saltwater pipe

Test specimen: strip.

Key Words: Cupronickel with Chromium
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.94 g/ccC71500
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 101
Tensile Strength, Ultimate 835 MPa
Tensile Strength, Yield 800 MPa
@Strain 0.2 %
Elongation at Break 6.0 %In 50 mm
Modulus of Elasticity 150 GPa
Poissons Ratio 0.271
Machinability 20 %Based on Free cutting brass = 100%
Shear Modulus 59.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000395 ohm-cm
@Temperature 20.0 °C
Magnetic Permeability 1.0003
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.8 µm/m-°C
@Temperature 20.0 - 200 °C
 17.1 µm/m-°C
@Temperature 20.0 - 300 °C
Thermal Conductivity 29.0 W/m-K
 29.2 W/m-K
@Temperature 100 °C
Mill Annealed (C71500)
 34.1 W/m-K
@Temperature 200 °C
Mill Annealed (C71500)
 38.6 W/m-K
@Temperature 300 °C
Mill Annealed (C71500)
 43.1 W/m-K
@Temperature 400 °C
Mill Annealed (C71500)
 48.1 W/m-K
@Temperature 500 °C
Mill Annealed (C71500)
 53.1 W/m-K
@Temperature 600.0 °C
Mill Annealed (C71500)
 58.1 W/m-K
@Temperature 700.0 °C
Mill Annealed (C71500)
Melting Point 1170 - 1220 °C
Solidus 1170 °C
Liquidus 1220 °C
 
Processing PropertiesOriginal ValueComments
Hot-Working Temperature 900 - 1065 °C
 
Component Elements PropertiesOriginal ValueComments
Beryllium, Be 0.50 %
Copper, Cu 67.8 %
Iron, Fe 0.70 %
Nickel, Ni 31 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nickel silver 65-10, UNS C74500, H02 Temper flat products
Copper Nickel Tin, UNS C72800
Copper nickel 10%, UNS C70600, OSO50 Temper flat products
Copper nickel 10%, UNS C70600, OSO35 Temper flat products
Copper nickel 10%, UNS C70600, OSO25 Temper flat products

MC71900b4 / 11761

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.