MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Saint-Gobain CHR® 2345-2 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape
Categories: Polymer; Tape; Thermoset; Polyimide, TS; Silicone

Material Notes: CHR® 2345-2 is manufactured from polyimide film with high-temperature adhesive.

Features/Benefits: CHR® 2345-2 has excellent mechanical and electrical properties as well as a high conformability. CHR® 2345-2 offers outstanding resistance to cut through and are impact and abrasion resistant. They also offer excellent dielectric strength, while the burning of the adhesive forms a non-conductive ash. CHR® 2345-2 meets the Underwriters Laboratories, Inc. Guide OANZ2 and File E51201 and File E66639 specifications respectively with a 180°C temperature rating, and it complies with UL510 for a flame retardant. Acrylic adhesive can be thermoset. The polyimide backing meets MIL-P-46112B.

Applications: CHR® 2345-2 is chosen for gold finger protection during wave solder applications.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 75 %75 %
Tear Strength 8.77 kN/m50.0 pliInitial Tear Strength
Peel Strength 0.270 kN/m1.54 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Breakdown 10000 V10000 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorAmber

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics METALKLIP® Clip-On EMI Gasket
P & P Technology Oriented Wires In Silicone
P & P Technology Monex Expanded Monel Foil
Norplex-Micarta P95 Polyimide Glass Laminate Sheet
Norplex-Micarta NP512 Epoxy Glass Laminate Sheet

PSTGQZ329 / 68843

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.