MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Omnix® DW-4050 Polyamide, High Performance (HPPA), 50% Glass Fiber  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 50% Glass Fiber Reinforced

Material Notes: Omnix® DW-4050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture absorption.

Omnix® DW-4050 is characterized by high stiffness and strength, very good impact properties, good dimensional stability and high flow properties. This material is an economical alternative for food service applications using die-cast alloys.

Omnix® DW-4050 is cleared for use under United States Food and Drug Administration (FDA) Conditions of Use B through H, in contact with all food types except Food Type VI C, Beverages containing more than 8 percent alcohol.

Omnix® DW-4050 is also cleared for food contact use by European Union regulations.

It processes readily using conventional injection molding machines and methods. Water-cooled molds are suitable for use with this grade.
- Black: Omnix® DW-4050 BK 001

Key Attributes: Fast Molding Cycle; Good Dimensional Stability; Good Impact Resistance; Good Surface Finish; High Flow; High Stiffness; High Strength; Hot Water Moldability; Paintable

Applications: Appliances; Food Service Applications

Agency Ratings: ACS Unspecified Rating; DVGW W270; EU Food Contact, Unspecified Rating; FDA Food Contact, Unspecified Rating; KTW Guidelines; NSF STD-51; WRAS Unspecified Rating

- Typical values shown tested on Dry as Molded samples.
- Standard Packaging and Labeling: Omnix® DW-4050 resin is packaged in foil lined, multiwall paper bags containing 25 kg (55 pounds) of material. Individual packages will be plainly marked with the p

Injection Notes: Drying:
- Omnix® DW-4050 resin is shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. Manufacturer recommends drying prior to molding. It should be dried before molding because excessive moisture content will result in reduced mechanical properties and processing issues, such as excessive nozzle drooling, foaming and splay visible on the molded parts.
- Recommended drying conditions are as follows:
-- Type of drier: Desiccant
-- Temperature: 80°C (175°F)
-- Time: 4-12 hours
-- Dew point: -30°C (-22°F) or lower
-- Polyamides oxidize in the presence of oxygen at high temperatures. Therefore drying temperatures above 80°C should be avoided, particularly for light colors or color-controlled parts.

Injection Molding:
- Omnix® DW-4050 resin can be readily injection molded in most screw injection molding machines. A general purpose screw is recommended, with minimum back pressure. The melt temperature should be between 275°C and 290°C (527°F and 554°F). Generally this can be achieved with barrel temperatures from 250°C (482°F) in the rear zone gradually increasing to 285°C (545°F) in the front zone. Mold temperature should be between 80° and 140°C (176° and 284°F).
- Set injection pressure to give rapid injection. Adjust holding pressure to one-half injection pressure. Set hold time to maximize part weight. Transfer from injection to hold pressure at the screw position just before the part is completely filled.

Storage:
- Omnix® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Omnix® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Omnix® processing guide.

Data for dry samples unless noted.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.59 g/cc0.0574 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0010 cm/cm0.0010 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.0050 cm/cm0.0050 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  205 MPa
@Temperature 23.0 °C
29700 psi
@Temperature 73.4 °F
Conditioned; ISO 527-2
 245 MPa
@Temperature 23.0 °C
35500 psi
@Temperature 73.4 °F
ISO 527-2
Elongation at Break  2.6 %
@Temperature 23.0 °C
2.6 %
@Temperature 73.4 °F
Conditioned; ISO 527-2
 2.6 %
@Temperature 23.0 °C
2.6 %
@Temperature 73.4 °F
ISO 527-2
Tensile Modulus  17.0 GPa
@Temperature 23.0 °C
2470 ksi
@Temperature 73.4 °F
Conditioned; ISO 527-2
 17.0 GPa
@Temperature 23.0 °C
2470 ksi
@Temperature 73.4 °F
ISO 527-2
Flexural Strength 350 MPa50800 psiISO 178
Flexural Modulus 15.0 GPa2180 ksiISO 178
Izod Impact, Notched (ISO)  15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 180
 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Izod Impact, Unnotched (ISO)  85.0 kJ/m²
@Temperature 23.0 °C
40.4 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 180
 90.0 kJ/m²
@Temperature 23.0 °C
42.8 ft-lb/in²
@Temperature 73.4 °F
ISO 180
Charpy Impact Unnotched  9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
 10.0 J/cm²
@Temperature 23.0 °C
47.6 ft-lb/in²
@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched  1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °FISO 11357-3
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 250 °C482 °F
Front Barrel Temperature 285 °C545 °F
Melt Temperature 275 - 290 °C527 - 554 °F
Mold Temperature 80.0 - 140 °C176 - 284 °F
Drying Temperature 80.0 °C
@Time 14400 - 43200 sec
176 °F
@Time 4.00 - 12.0 hour
 
Descriptive Properties
Availability (as of March 2019)Asia Pacific; Europe; North America
ColorBlack
FormsPellets
Part Marking Code [ISO 11469]>(PA+PPA)-GF50<
ProcessingInjection Molding; Water-Heated Mold Injection Molding
RoHS ComplianceRoHS Compliant

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y5255 / 238636

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.