MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Elkem Silicon Injection Grade
Categories: Metal; Nonferrous Metal

Material Notes: Silicon Injection Grade is a refined, fine sized silicon product in the range 0,5-3 mm with max 15 % -0,5 mm.

The main application for Silicon Injection Grade is as alloying element in aluminum. Silicon Injection Grade can be injected or added through a metallic pump into liquid aluminum.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Particle Size 500 - 3000 µm
 
Component Elements PropertiesOriginal ValueComments
Calcium, Ca <= 0.050 %
Iron, Fe <= 0.45 %
Silicon, Si >= 98 %
Titanium, Ti 0.020 - 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon Carbide, CVD
Master Bond MasterSil 922-LO Silicone
Advanced Elastomer Systems Santoprene® 253-50 Thermoplastic Rubber
Bamberger Polymers Bapolene® EVA-1120 Ethylene Vinyl Acetate (EVA)
Dow 1250 SURFACTANT

NELKEM11 / 16169

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.