MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

SunChemical Gwent C2030922D1 Silver Ink
Categories: Fluid; Metal; Other Engineering Material; Ceramic/Metallic Coating

Material Notes: Silver Ink C2030922D1 is a grey ink with a pine smell at a ready to use viscosity suitable for firing on glass and ceramic to form conductive tracks. The ink should be gently stirred before use avoiding introduction of air bubbles.
Silver Ink has a low resistance ink designed for use as the heating bars and tracks on automobile backlights and other circuits on glass. It has a dark back color when printed and fired on float side of glass. It can be printed onto IR or UV black enamels.
Screen Printing Equipment: semi-automatic, automatic
Screen Types: stainless steel, polyester, mesh 156-325 tpi
Substrate: Glass

Information provided by Gwent Electronic Materials Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 84 - 86 %
@Temperature 700 °C
84 - 86 %
@Temperature 1290 °F
Viscosity 3000 - 5500 cP
@Shear Rate 230 1/s,
Temperature 25.0 °C
3000 - 5500 cP
@Shear Rate 230 1/s,
Temperature 77.0 °F
Haake VT 550 PK1.1°
Storage Temperature 20.0 °C68.0 °Fsealed container
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square  0.015 - 0.020 ohm
@Thickness 0.0250 mm
0.015 - 0.020 ohm
@Thickness 0.000984 in
Printed onto 125µm PET film
 0.030 - 0.045 ohm
@Thickness 0.0100 mm
0.030 - 0.045 ohm
@Thickness 0.000394 in
Printed onto 125µm PET film
 
Processing PropertiesMetricEnglishComments
Sintering Temperature 550 - 750 °C1020 - 1380 °F
Cure Time 15.0 min
@Temperature 150 °C
0.250 hour
@Temperature 302 °F
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
Bending TestInk survived 3 cyclesPrinted onto 125µm PET film, Failure at resistance 10 times the initial value using 2kg weight.
Coverage cm2/g110Using a 230 mesh stainless steel screen
Double CuringAging factor of -0.7% after double curing at 150C for 15 mins.Printed onto 125µm PET film
Hot Water TestAging factor of -0.2% after boiling for 1 hr.Printed onto 125µm PET film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
SunChemical Gwent C2030701D3 Solderable Silver Ink
SunChemical Gwent C2100203D2 Silver Ink
SunChemical Gwent C2090819P2 Silver Ink
SunChemical Gwent C2090210P12 Silver Ink
SunChemical Gwent C2050712D58 Silver Ink for ITO Substrates

WGELZ9076 / 139389

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.