MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
INEOS Styrolution Terluran® GP-35 ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Material Notes: Terluran® GP-35 is high-flow, general purpose injection molding grade with good ductility, intended for moldings with thin walls and/or adverse flow length to wall ratio. Excellent colorability, High flowability, Good impact resistance, Good heat distortion resistance, High quality surface finish and gloss, Great mechanical strength and rigidity.

Applications: Injection molding, Thin wall components for telecommunications, Household and sanitary appliances, Toys, Automotive components, Electroplating.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccISO 1183
Moisture Absorption at Equilibrium 0.24 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.95 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cmISO 294-4
Melt Flow 34 g/10 min
@Load 10.0 kg,
Temperature 220 °C
Volumetric; cm3/10 min; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ASTM Test
Ball Indentation Hardness 99.0 MPaISO 2039-1
Tensile Strength, Yield 44.0 MPaISO 527
Elongation at Break 12 %Nominal; ISO 527
 >= 15 %ISO 527
Elongation at Yield 2.4 %ISO 527
Tensile Modulus 2300 MPaISO 527
Flexural Strength 65.0 MPaISO 178
Izod Impact, Notched 80.0 J/m
@Temperature -30.0 °C
ASTM Test
 85.0 J/m
@Temperature -18.0 °C
ASTM Test
 2.40 J/cm
@Thickness 3.17 mm
ASTM Test
Izod Impact, Notched (ISO) 7.00 kJ/m²
@Temperature -30.0 °C
ISO 180/A
 22.0 kJ/m²
@Temperature 23.0 °C
ISO 180/A
Charpy Impact Unnotched 90.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eU
 125 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 7.00 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 19.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+13 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 - 110 µm/m-°CISO 11359
Thermal Conductivity 0.170 W/m-KDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °Cannealed 4 hours at 80°C; ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 92.0 °Cannealed 4 hours at 80°C; ISO 75
Vicat Softening Point 95.0 °C
@Load 5.10 kg
VST/B/50. 50C/h; ISO 306
 102 °C
@Load 1.02 kg
VST/A/50. 50C/h; ISO 306
 
Optical PropertiesOriginal ValueComments
Yellow Index 13 %DIN 6167
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °CISO 294
Mold Temperature 30.0 - 80.0 °CISO 294
Injection Velocity 200 mm/secISO 294
Drying Temperature 80.0 °C
@Time 7200 - 14400 sec
 
Compliance PropertiesOriginal ValueComments
FDA Yes
NSF YesNSF Std. 14
 YesNSF Std. 51
 YesNSF Std. 61
USP Class VI No
 
Descriptive Properties
ColorNatural
Commercial StatusNorth America and Europe
FormPellets
Impact ModifiedYes
Primary Processing TechniqueInjection Molding
ProcessingInjection Molding
Special characteristicPlatable
UL.UL-CYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
INEOS Styrolution Terluran® GP-22 ABS
Lotte Advanced Materials Starex® HG-0760 ABS, Unreinforced
Elix Polymers Elix™ P2H-AT ABS Polymer
Lotte Advanced Materials Starex® HF-0660I ABS, Unreinforced
Lotte Advanced Materials Starex® SD-0150 ABS, Unreinforced

PBASF9050 / 84814

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.