Characteristics: Ammonia free Increased CTI High electrical insulation properties High mechanical strength Temperature stability (230 0 C) Color-black Medium flow Applications: Switchgear componentCommutators (washing machine, motors, vacuum cleaner, electrical tools and large commutators )Automotive components ( electrical ), etc.
Information provided by Amity Thermosets Limited |