MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Resirene Biorene® HA-25 Thermoplastic Starch - Polystyrene Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS)

Material Notes: Thermoplastic Starch / Polystyrene Hybrid Resin. Features: 25% Thermoplastic Starch (biodegradable according to ISO 20200:2015), Easy to Process, Lower temperature profile, FDA Compliant.

Applications: Extrusion Foams, Disposable/Single-use trays, Ready-to-eat food containers.

This bio-based starch-based resin is an option to replace traditional resins such as Polypropylene (PP), Polyethylene (PE) and Polystyrene (PS) for single-use applications and / or packaging products. All Biorene® grades are “OK biobased” certified, offered by TÜV AUSTRIA.

Information provided by Resirene

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Melt Flow  1.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 2.5 g/10 min
@Load 2.16 kg,
Temperature 230 °C
2.5 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 38.0 MPa5510 psiASTM D638
Elongation at Break 5.0 %5.0 %ASTM D638
Flexural Modulus 2.48 GPa360 ksiASTM D638
Izod Impact, Notched 0.100 J/cm
@Thickness 3.17 mm
0.187 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Processing PropertiesMetricEnglishComments
Processing Temperature <= 220 °C<= 428 °F
Rear Barrel Temperature 160 - 170 °C320 - 338 °FExtrusion
Middle Barrel Temperature 175 - 185 °C347 - 365 °FExtrusion
Front Barrel Temperature 190 - 200 °C374 - 392 °FExtrusion
 
Compliance PropertiesMetricEnglishComments
FDA YesYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRESIR919 / 250140

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.