MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Konson Accelerator TBzTD-80 Masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Composition: 80 % tetrabenzylthiuram disulphide, 20% EPDM/EVA binder and dispersing agents

Use Characteristics: Konson®TBzTD-80 accelerates the vulcanization of natural and synthetic rubbers with a high level of processing safety. Konson®TBzTD-80 forms no carcinogenic nitrosamines within the definition of TRGS 552. The addition of mercapto or sulfenamide accelerators slows the vulcanization process. Scorch and vulcanization times are reduced. The degree of cross- linking is not greatly affected. Basic accelerators such as aldehyde-amine and guanidine have an additional activating effect. Konson®TBzTD-80 is used as a primary accelerator in the presence of sulfur, as a secondary accelerator with thiazoles and as a sulfur-free vulcanizing agent. Cross-linking without free sulfur or lowsulfur cross-linking produces extremely heat-resistant vulcanizates with good aging characteristics.

Processing Advantages: The thermoplastic, excellent compatible EPDM/EVA binder which is combined with active dispersing promoters allows much more easily and quickly incorporation and excellent dispersion in the rubber mixing. In this way, optimal activity of the effective TBzTD is assured.

Dosage levels: Primary( in technical rubber articless) : 0.2 – 2.0 phr Konson®TBzTD-80 and 0.9 – 2.8 phr Konson®S-80; Secondary: 0.2 – 0.5 phr Konson®TBzTD-80 and 1.1 – 1.6 phr MBTS-75; Without free sulfur (for heat resistance compounds): 2.4 – 3.8 phr Konson®TBzTD-80 and 0.53 – 1.1 phr Konson®MBTS-75.

Applications: Heat-resistant technical articles, cable sheathing and insulation, hard rubber, etc.

Information provided by Konson®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.16 g/cc0.0419 lb/in³
Ash <= 0.30 %<= 0.30 %
Evaporation Loss <= 0.30 %<= 0.30 %
 
Thermal PropertiesMetricEnglishComments
Melting Point 130 °C266 °F
 
Descriptive Properties
Appearancebeige granules
Content= 96%TBzTD
Sieve residue= 0.3 %63µm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKONS004 / 256049

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.