MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

RA-333 Nickel Alloy (UNS N06333)
Categories: Metal; Nonferrous Metal; Nickel Alloy

Material Notes: Used for turbine parts, radiant tubes.

Property data for annealed samples.

Key Words: ATG 33
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.24 g/cc0.298 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Rupture Strength  6.21 MPa
@Temperature 1090 °C,
Time 3.60e+6 sec
900 psi
@Temperature 2000 °F,
Time 1000 hour
 11.0 MPa
@Temperature 1090 °C,
Time 360000 sec
1600 psi
@Temperature 2000 °F,
Time 100 hour
 14.5 MPa
@Temperature 982 °C,
Time 3.60e+6 sec
2100 psi
@Temperature 1800 °F,
Time 1000 hour
 28.3 MPa
@Temperature 982 °C,
Time 360000 sec
4100 psi
@Temperature 1800 °F,
Time 100 hour
 58.6 MPa
@Temperature 816 °C,
Time 3.60e+6 sec
8500 psi
@Temperature 1500 °F,
Time 1000 hour
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.2 µm/m-°C
@Temperature 20.0 - 100 °C
7.89 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 12.6 W/m-K
@Temperature 20.0 - 100 °C
87.0 BTU-in/hr-ft²-°F
@Temperature 68.0 - 212 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.050 %0.050 %
Chromium, Cr 25 %25 %
Cobalt, Co 3.0 %3.0 %
Iron, Fe 18 %18 %
Molybdenum, Mo 3.0 %3.0 %
Nickel, Ni 45 %45 %
Tungsten, W 3.0 %3.0 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wall Colmonoy COLMONOY® 635 Nickel-Chromium-Boron Matrix Alloy With Tungsten Carbide
IN-102 Nickel Alloy, UNS N06102
Overview of materials for Nickel Alloy
MetalTek MTEK N-12MV Cast UNS N30012 Severe Corrosion and Heat Resistant Alloy
Universal Wire Works Nichrome V (AMS 5676) Nickel Alloy Filler Metal

MN996 / 150615

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.