This off-white paste epoxy is a versatile adhesive systems. The choice of one of four recommended Activators (A, E, W or H-20) makes A-2 Adhesive an ideal choice for many applications. A-2 with Activators W or H-20 has a very low thermal expansion coefficient, especially important for bonding ceramics, porcelain, etc. A-2 with Activator A is qualified under Mil. Spec. MIL-A-47284 (MI). Information provided by Ellsworth Adhesives. |