MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Dover Chemical MAYCO BASE 1217LV Highly Sulfurized Fatty Oil, Staining Sulfurized Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Mayco Base 1217LV is a highly sulfurized, low viscosity fatty material. The additive’s low viscosity allows the metalworking blender to bypass heated storage, usually mandatory in dealing with most fortified sulfurized additives. Mayco Base 1217LV is not recommended for use in products destined for applications on any yellow metal (copper, brass & bronze), due to its high level of activity. Also, it is recommended the additive be incorporated in naphthenic oil-based products, as opposed to paraffinic-oil based products.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.03 g/cc
@Temperature 15.6 °C
1.03 g/cc
@Temperature 60.0 °F
60/60°F
Density 1.02 g/cc0.0368 lb/in³
Saybolt Viscosity at 210°F 350 SUS350 SUS
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 5.05.0[meqKOH/g]
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 204 °C>= 399 °FCOC
 
Component Elements PropertiesMetricEnglishComments
Sulfur, S 6.0 %6.0 %Active
 18 %18 %Total
 
Descriptive Properties
AppearanceDark Brown Fluid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

WDOVER107 / 217726

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.